The alloy (60% Bi, 40% Cd) called eutectic alloy shows that solidification starts and is completed
A. for range of temperature 321°C to 144°C
B. at a single temperature of 144°C
C. at a single temperature of 271°C
D. at a single temperature of 321°C
Answer: Option B