Ductile cast iron
A. Contains 1.7 to 3.5% carbon in Free State and is obtained by the slow cooling of molten cast iron
B. Is also known as chilled cast iron and is obtained by cooling rapidly. It is almost unmachinable
C. Is produced by annealing process. It is soft, tough and easily machined metal
D. Is produced by small additions of magnesium (or creium) in the ladle. Graphite is in nodular or spheroidal form and is well dispersed throughout the material
Answer: Option D
Solution(By Examveda Team)
Ductile cast iron Is produced by small additions of magnesium (or creium) in the ladle. Graphite is in nodular or spheroidal form and is well dispersed throughout the materialductile iron has much more impact and fatigue resistance, due to its nodular graphite inclusions.
Related Questions on Engineering Materials
Manganese is added in low carbon steel to
A. Make the steel tougher and harder
B. Raise the yield point
C. Make the steel ductile and of good bending qualities
D. All of the above
The elastic stress strain behavior of rubber is
A. Linear
B. Nonlinear
C. Plastic
D. No fixed relationship