A liquid phase sintered SiC-Ni composite has a solid-solid grain boundary energy (γSiC-SiC) of 0.80 J.M-2 and a solid-liquid (γSiC-SiC) interfacial energy of 0.45 J.m-2. For a SiC grain size of 20 μm, the average interparticle (SiC-SiC) neck size (in μm) is:
A. 3.03
B. 4.28
C. 9.16
D. 18.32
Answer: Option C

Join The Discussion