Match the defect with appropriate cause.
List-I List-II
P. Hot tear 1. Inadequate riser
Q. Porosity 2. Loosely rammed sand mould
R. Sand inclusions 3. Mould restraint
S. Shrinkage cavity 4. Gas entrapment

A. P-3, Q-2, R-4, S-1

B. P-3, Q-2, R-1, S-4

C. P-1, Q-4, R-2, S-3

D. P-4, Q-3, R-2, S-1

Answer: Option A


This Question Belongs to Metallurgical Engineering >> Foundry Metallurgy