In full annealing, the hypo eutectoid steel is heated from 30°C to 50°C above the upper critical temperature and then cooled
A. In still air
B. Slowly in the furnace
C. Suddenly in a suitable cooling medium
D. Any one of these
Answer: Option B
Solution(By Examveda Team)
In full annealing, the hypo eutectoid steel is heated from 30°C to 50°C above the upper critical temperature and then cooled Slowly in the furnaceRelated Questions on Engineering Materials
Manganese is added in low carbon steel to
A. Make the steel tougher and harder
B. Raise the yield point
C. Make the steel ductile and of good bending qualities
D. All of the above
The elastic stress strain behavior of rubber is
A. Linear
B. Nonlinear
C. Plastic
D. No fixed relationship