The grain size of pure copper after annealing for 103S is 10 μm. If the time exponent is 0.5, the total time of annealing required to obtain a grain size of 40 μm is . . . . . . . . S.
A. 4 × 103
B. 8 × 103
C. 16 × 103
D. 64 × 103
Answer: Option C
Related Questions on Physics of Metals in Metallurgy
When the wavelength of the incident X-Tay increases the angle of diffraction
A. decreases
B. increases
C. remains constant
D. shows no systematic variation
A. Burger vector and the dislocation line are Parallel to each other for screw dislocations
B. Burger vector and the dislocation line are perpendicular to each other for edge dislocations
C. Screw dislocations glide parallel to its Burger vector
D. Edge dislocations glide parallel to its Burger Vector