Chilled cast iron. Iron-carbon alloy with low graphitization factor so that chill occurs forming a graphite-free structure.
In order to achieve chilling, the silicon content is set to a low level depending on the wall thickness of the casting; the carbon content is approx. 2.5 to 3.8%.
In order to achieve chilling, the silicon content is set to a low level depending on the wall thickness of the casting; the carbon content is approx. 2.5 to 3.8%.